Sign In | Join Free | My polstate.com |
|
Brand Name : XUNSHI
Model Number : UNS K94840
Certification : ISO9001:2015
Place of Origin : China
MOQ : 150 kg
Price : Negotiable
Payment Terms : T/T
Supply Ability : 10 ton per month
Delivery Time : 30 days
Packaging Details : Plywood crate
Equal grade : 1.3922, K94840
Trade name : HIGH PERMEABILITY 49, IMPHY® SUPRA 50, FeNi48
Spec : ASTM A753, ASTM F30
K94840 is a 48% nickel-iron alloy that possesses the highest saturation flux density of any nickel-iron alloy. The saturation flux density of about 16000 gauss (1.6 Tesla) combined with high magnetic permeability and low core loss makes this a versatile alloy with many potential applications.
K94840 has been used in laminated cores for instrument transformers, magnetic shields and cores for certain electronic and communications devices in which extremely high permeability at low magnetizing forces greatly increases the efficiency and effectiveness of the equipment.
Because of its high permeability, it has also been used in solenoid cores and sensitive relays that must respond to low magnetizing forces
Chemical composition
Element | C | Mn | Si | P | S | Cr | Ni | Mo | Co | Cu | Fe |
Wt, % | 0.05 | 0.80 | 0.50 | 0.03 | 0.01 | 0.30 | 47-49 | 0.30 | 0.50 | 0.30 | rem |
Key Properties:
Applications
Specs
Heat treatment
Standard hydrogen anneal
For maximum softness and optimum magnetic and electrical properties, K94840 should be annealed in an oxygen-free, dry hydrogen atmosphere with a dew point below -40°F (-40°C) for 2 to 4 hours at 2150°F (1177°C), followed by a furnace cool at a rate of 100/200°F (55/110°C) per hour down to 800°F (427°C) and at any rate thereafter.
Oil, grease, lacquer, and any other contaminants must be removed before annealing. During hydrogen annealing, the individual parts should be separated by a surface insulation media or an inert insulating powder, such as magnesium or aluminum oxide.
![]() |
K94840 Iron-Nickel Soft Magnetic Alloy Highest SaturationFlux Density FeNi Alloy Images |